NCF800
video
NCF800

NCF800 - Superalloys

Products Description Chemical composition Mechanical Properties In terms of mechanical properties, NCF800 exhibits good tensile strength and ductility. It can withstand heavy loads and mechanical stresses without succumbing to brittle failure. This combination of strength and flexibility allows...

Description
Products Description

 

 

 Chemical composition 

C
≤
Si
≤
Mn
≤
P
≤
S
≤
Cr Ni
0.1 1.0 1.5 0.03 0.015 19-23 30-35
Mo Al Cu Nb Ti V Fe
  0.15-0.6 0.75   0.15-0.6   ...
N Co Pb B Other    
             
             

 

Mechanical Properties

Properties Conditions
T (°C) Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 1158 25 oil quenched, fine grained, tempered at 425°C
Yield Strength (Mpa) 1034
Elongation (%) 15
Reduction in Area (%) 53
Hardness (HB) 335 25 oil quenched, fine grained, tempered at 425°C

 

In terms of mechanical properties, NCF800 exhibits good tensile strength and ductility. It can withstand heavy loads and mechanical stresses without succumbing to brittle failure. This combination of strength and flexibility allows for the fabrication of complex and durable structures. Moreover, the alloy has excellent creep resistance, which means it can maintain its shape and dimensions under long-term exposure to high temperatures and constant stress. This is crucial for applications where dimensional stability is essential, such as in gas turbines and steam boilers.

201908211429116655414

The fabricability of NCF800 is another advantage. It can be easily processed through various manufacturing techniques, including casting, forging, and machining. This enables the production of customized components with precise geometries and high-quality finishes. Additionally, the alloy has good weldability, facilitating the assembly of large structures and the repair of damaged parts.

 

Overall, NCF800 superalloys offer a unique blend of high-temperature resistance, mechanical strength, and fabricability. Their reliability and performance in harsh conditions make them indispensable in modern industrial sectors, driving innovation and ensuring the efficient and safe operation of many critical systems.