GL-A36 Steel Plate
Products Description During the welding process, it is crucial to identify and handle welding defects in a timely and correct manner to ensure welding quality. The following are the identification and handling methods for common welding defects: I. Identification of Welding Defects (A)...
Description
Products Description
During the welding process, it is crucial to identify and handle welding defects in a timely and correct manner to ensure welding quality. The following are the identification and handling methods for common welding defects:
I. Identification of Welding Defects
(A) Appearance Defects
Undercut
Identification Method: Undercut refers to the groove left on the base metal after it is melted by the electric arc along the edge of the weld. It can usually be detected by visual inspection, appearing as a concave part on the edge of the weld that is lower than the surface of the base metal, with an irregular shape and varying depths and lengths. When inspecting, special attention should be paid to the junction between the weld and the base metal, especially when the welding speed is relatively fast, the welding current is relatively large, or the arc is too long, as undercut is prone to occur in these situations.
Porosity
Identification Method: Porosity is the cavity left in the weld when the gas in the molten pool fails to escape during solidification. In appearance, porosity may be round, oval, or elongated, and varies in size. Some pores are clearly visible on the surface of the weld, presenting as smooth small holes; while some may be hidden inside the weld and can only be detected by non-destructive testing means. Generally, porosity is likely to occur when the welding protection is poor (such as insufficient gas flow in gas-shielded welding, or wet electrodes in manual arc welding) or when excessive gas is generated during the metallurgical reaction of the molten pool.
Slag Inclusion
Identification Method: Slag inclusion refers to the residual slag in the weld. On the surface of the weld, slag inclusion appears as black or gray dotted, striped, or blocky impurities. These impurities do not have a metallic luster and are clearly distinguishable from the surrounding weld metal. They can be observed by visual inspection or with a low-power magnifying glass. Slag inclusion is mainly caused by incomplete slag removal during the welding process (such as uncleaned inter-pass slag in multi-pass and multi-layer welding) or by a too-small welding current, which results in the slag not being able to float out of the molten pool fully.
Lack of Fusion
Identification Method: Lack of fusion refers to the part where the weld metal and the base metal or between different weld metals are not completely melted and combined. During visual inspection, the transition between the weld in the lack-of-fusion area and the surrounding normal weld is unnatural, and there may be an obvious dividing line. Also, the surface of the weld in the lack-of-fusion area may appear slightly concave. This defect usually occurs when the welding parameters are improper (such as too-fast welding speed, too-small welding current) or when the groove is not cleaned thoroughly.
Weld Bead
Identification Method: A weld bead is the metal lump formed when the molten metal flows onto the unmelted base metal outside the weld during the welding process. It forms a protruding part on the surface of the weld, with an irregular shape and varying sizes depending on the welding conditions. Weld beads are mainly caused by a too-large welding current, too-slow welding speed, or inappropriate groove dimensions, which lead to excessive molten pool metal that cannot be controlled from flowing.
(B) Internal Defects
Crack
Identification Method: Cracks are the most dangerous type of welding defects and may appear on the surface or inside the weld. Surface cracks can be detected by visual inspection or with the help of magnetic particle testing (for magnetic materials) and penetrant testing (for non-magnetic materials). Surface cracks are generally straight or dendritic, with obvious gaps and a darker color. Internal cracks need to be identified by non-destructive testing means such as ultrasonic testing and radiographic testing, appearing as continuous or discontinuous black lines on the test images. The occurrence of cracks is usually related to factors such as excessive welding stress, poor quality of welding materials, and unreasonable welding processes.
Incomplete Penetration
Identification Method: Incomplete penetration refers to the phenomenon that the root of the joint is not completely penetrated during welding. For butt welds, incomplete penetration can be identified by observing whether there is a continuous lack-of-fusion area at the root of the weld. Incomplete penetration may show certain signs on the surface of the weld, such as a narrow root of the weld and discontinuous fusion lines. However, accurate judgment usually requires the use of ultrasonic testing or radiographic testing methods, appearing as black lines or dark areas at the root of the weld in the test results. Incomplete penetration is mainly caused by a too-small welding current, too-small groove angle, too-thick root face, or too-fast welding speed.
|
GL-A36 high Strength Chemical Composition in Tempering and Quenching |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
GL-A36 |
0.18 |
0.50 |
0.90-1.6 |
0.035 |
0.035 |
0.015 |
|
|
Nb |
V |
Ti |
Cu |
Cr |
Ni |
Mo |
|
|
0.02-0.05 |
0.05-0.10 |
0.02 |
0.30 |
0.2 |
0.4 |
0.08 |
|




Why Choose Us?
We take pride in our ability to provide custom solutions for our customers' unique needs.
We analyze and compare the previous products and the current technical situation of our GL-A36 Steel Plate, and develop new technical specifications and processes.
Our customers trust us to deliver high-quality Cold-rolled Steel products on time and on budget.
We strictly implement the warm and thoughtful after-sales service, adhere to the development of good professional ethics.
We offer a wide range of Cold-rolled Steel products to meet diverse customer needs.
We adhere to the customer-centric and brand-oriented business philosophy, and continue to provide customers with reliable and excellent products and services.
Our factory is committed to upholding the highest standards of safety and quality.
All staff of our company and all departments work together to combine business management, professional technology, quantitative statistical methods and ideological education.
Our Cold-rolled Steel products are known for their durability and reliability.
Relying on the superior conditions and strong advantages of mass production, we are able to meet the different needs of our customers.
Hot Tags: gl-a36 steel plate, China gl-a36 steel plate suppliers, factory, 1 4401, C62300, C6161, 1 441, CuZn38Pb2, HX340BD